Plantation Timber, the true renewable resource

Wespine Blue - Test Results

Wespine Blue has been extensively tested over a three year period by respected organisations such as the CSIRO. The results of this testing conclude that Wespine Blue forms a treatment envelope of 5mm average depth with specified levels of active constituent which is effective in protecting framing timbers against termite attack.

Wespine Blue Treatment Uptake and Confirmation of Envelope

Timber

Uptake L/m3

STD Dev

Radiata heartwood

10

3.5

Radiata sapwood

15

3.5

Slash heartwood<

8

5.3

Slash sapwood

15

2.9

 

Wespine Blue Does Not Negatively Affect Important Wood Properties

Property

Method of Test

Result

Strength- MOR and MOE

AS4063

No different to matched untreated samples

Nailplate withdrawal

AS1649

No different to matched untreated samples

Adhesion (plasterboard)

AS2753

No deleterious effect on adhesion

Corrosion of metal in contact with treated wood

AWPA E12-94

Non-corrosive

Paintability

Wattyl - Paint industry standard adhesion test

No affect on adhesion. Very slight affect on gloss levels with 2 products tested

Ignitability

AS1530.1

No different from untreated controls







If you require technical assistance contact Wespine's Technical Desk on Free Call 1800 018 888
Wespine is a Wholesaler of pine products, contact one of our Distributors for product availability and pricing. Click here for Distributor locations.